Multi-method characterization of soda-lime glass corrosion : Part 1. Analysis techniques and corrosion in liquid water Report of the International Commission on Glass (ICG) Subcommittee of Technical Committee 19 "Glass Surface Diagnostics"

Loading...
Thumbnail Image

Date

Editor

Advisor

Volume

74

Issue

Journal

Glass Science and Technology

Series Titel

Book Title

Publisher

Offenbach : Verlag der Deutschen Glastechnischen Gesellschaft

Supplementary Material

Other Versions

Link to publishers' Version

Abstract

Corroded soda-lime float glass surfaces prepared in water (room temperature and 60 °C) or air (relative humidity of 95 %, 60 °C) for different times are invesdgated by means of SIMS, SNMS, XPS, NRA, ERD, RBS, GIXR, AFM, SEM, light microscopy and scratch testing. The corrosion effects are studied for as-received and cleaned glass surfaces. Changes in the dement concentration in the glass interfaces with the immersion time in water are described. They are combined with variations in density of the surface layer which exhibits plastic deformation behaviour. Inhomogeneous corrosion leads to changes in the topography and an increase in surface roughness.

Description

Keywords

Keywords GND

Conference

Publication Type

Article

Version

publishedVersion

License

CC BY 3.0 DE