    The force of MOFs: The potential of switchable metal-organic frameworks as solvent stimulated actuators
    (Cambridge : RSC, 2020) Freund, Pascal; Senkovska, Irena; Zheng, Bin; Bon, Volodymyr; Krause, Beate; Maurin, Guillaume; Kaskel, Stefan
    We evaluate experimentally the force exerted by flexible metal-organic frameworks through expansion for a representative model system, namely MIL-53(Al). The results obtained are compared with data collected from intrusion experiments while molecular simulations are performed to shed light on the re-opening of the guest-loaded structure. The critical impact of the transition stimulating medium on the magnitude of the expansion force is demonstrated.
  • Item
    Influence of Polyvinylpyrrolidone on Thermoelectric Properties of Melt-Mixed Polymer/Carbon Nanotube Composites
    (Basel : MDPI, 2023) Krause, Beate; Imhoff, Sarah; Voit, Brigitte; Pötschke, Petra
    For thermoelectric applications, both p- and n-type semi-conductive materials are combined. In melt-mixed composites based on thermoplastic polymers and carbon nanotubes, usually the p-type with a positive Seebeck coefficient (S) is present. One way to produce composites with a negative Seebeck coefficient is to add further additives. In the present study, for the first time, the combination of single-walled carbon nanotubes (SWCNTs) with polyvinylpyrrolidone (PVP) in melt-mixed composites is investigated. Polycarbonate (PC), poly(butylene terephthalate) (PBT), and poly(ether ether ketone) (PEEK) filled with SWCNTs and PVP were melt-mixed in small scales and thermoelectric properties of compression moulded plates were studied. It could be shown that a switch in the S-value from positive to negative values was only possible for PC composites. The addition of 5 wt% PVP shifted the S-value from 37.8 µV/K to −31.5 µV/K (2 wt% SWCNT). For PBT as a matrix, a decrease in the Seebeck coefficient from 59.4 µV/K to 8.0 µV/K (8 wt% PVP, 2 wt% SWCNT) could be found. In PEEK-based composites, the S-value increased slightly with the PVP content from 48.0 µV/K up to 54.3 µV/K (3 wt% PVP, 1 wt% SWCNT). In addition, the long-term stability of the composites was studied. Unfortunately, the achieved properties were not stable over a storage time of 6 or 18 months. Thus, in summary, PVP is not suitable for producing long-term stable, melt-mixed n-type SWCNT composites.
  • Item
    Surface modification of MWCNT and its influence on properties of paraffin/MWCNT nanocomposites as phase change material
    (Hoboken, NJ [u.a.] : Wiley InterScience, 2020) Avid, Arezoo; Jafari, Seyed Hassan; Khonakdar, Hossein Ali; Ghaffari, Mehdi; Krause, Beate; Pötschke, Petra
    Multiwalled carbon nanotubes (MWCNTs) were modified by an organo-silane in order to improve their dispersion state and stability in paraffin wax. A family of paraffin-based phase change material (PCM) composites filled with MWCNTs was prepared with different loadings (0, 0.1, 0.5, and 1 wt%) of pristine MWCNTs and organo-silane modified MWCNTs (Si-MWCNT). Structural analyses were performed by means of Fourier transform infrared (FTIR), scanning electron microscopy (SEM), and rheological studies using temperature sweeps. Moreover, phase change transition temperatures and heat of fusion as well as thermal and electrical conductivities of the developed PCM nanocomposites were determined. The SEM micrographs and FTIR absorption bands appearing at approximately 1038 and 1112 cm−1 confirmed the silane modification. Differential scanning calorimetery (DSC) results indicate that the presence of Si-MWCNTs leads to slightly favorable enhancement in the energy storage capacity at the maximum loading. It was also shown that the thermal conductivity of the PCM nanocomposites, in both solid and liquid phases, increased with increasing the MWCNT content independent of the kind of MWCNTs by up to about 30% at the maximum loading of MWCNTs. In addition, the modification of MWCNTs made the samples completely electrically nonconductive, and the electrical surface resistivity of the PCMs containing pristine MWCNTs decreased with increasing MWCNTs loading. Furthermore, the rheological assessment under consecutive cyclic phase change demonstrated that the samples containing modified MWCNTs are more stable compared to the PCM containing pristine MWCNTs. © 2019 Wiley
  • Item
    Nitrogen-Doped Carbon Nanotube/Polypropylene Composites with Negative Seebeck Coefficient
    (Basel : MDPI, 2020) Krause, Beate; Konidakis, Ioannis; Arjmand, Mohammad; Sundararaj, Uttandaraman; Fuge, Robert; Liebscher, Marco; Hampel, Silke; Klaus, Maxim; Serpetzoglou, Efthymis; Stratakis, Emmanuel; Pötschke, Petra
    This study describes the application of multi-walled carbon nanotubes that were nitrogen-doped during their synthesis (N-MWCNTs) in melt-mixed polypropylene (PP) composites. Different types of N-MWCNTs, synthesized using different methods, were used and compared. Four of the five MWCNT grades showed negative Seebeck coefficients (S), indicating n-type charge carrier behavior. All prepared composites (with a concentration between 2 and 7.5 wt% N-MWCNTs) also showed negative S values, which in most cases had a higher negative value than the corresponding nanotubes. The S values achieved were between 1.0 µV/K and −13.8 µV/K for the N-MWCNT buckypapers or powders and between −4.7 µV/K and −22.8 µV/K for the corresponding composites. With a higher content of N-MWCNTs, the increase in electrical conductivity led to increasing values of the power factor (PF) despite the unstable behavior of the Seebeck coefficient. The highest power factor was achieved with 4 wt% N-MWCNT, where a suitable combination of high electrical conductivity and acceptable Seebeck coefficient led to a PF value of 6.1 × 10−3 µW/(m·K2). First experiments have shown that transient absorption spectroscopy (TAS) is a useful tool to study the carrier transfer process in CNTs in composites and to correlate it with the Seebeck coefficient.
  • Item
    Electrically conductive and piezoresistive polymer nanocomposites using multiwalled carbon nanotubes in a flexible copolyester: Spectroscopic, morphological, mechanical and electrical properties
    (Amsterdam [u.a.] : Elsevier, 2022) Dhakal, Kedar Nath; Khanal, Santosh; Krause, Beate; Lach, Ralf; Grellmann, Wolfgang; Le, Hai Hong; Das, Amit; Wießner, Sven; Heinrich, Gert; Pionteck, Jürgen; Adhikari, Rameshwar
    Nanocomposites of multiwalled carbon nanotubes (MWCNTs) with poly(butylene adipate-co-terephthalate) (PBAT), a flexible aromatic–aliphatic copolyester, were prepared by melt mixing followed by compression moulding to investigate their spectroscopic, morphological, mechanical and electrical properties. A comparison of the Fourier transform infrared (FTIR) spectra of the neat polymer matrix and the composites showed no difference, implying a physical mixing of the matrix and the filler. A morphological investigation revealed the formation of a continuous and interconnected MWCNT network embedded in the polymer matrix with partial agglomeration. Increasing Martens hardness and indentation modulus and decreasing maximum indentation depth with increasing filler concentration demonstrated the reinforcement of the polymer by the MWCNTs. A volume resistivity of 4.6 × 105 Ω cm of the materials was achieved by the incorporation of only 1 wt.-% of the MWCNTs, which confirmed a quite low percolation threshold (below 1 wt.-%) of the nanocomposites. The electrical volume resistivity of the flexible nanocomposites was achieved up to 1.6 × 102 Ω cm, depending on the filler content. The elongation at the break of the nanocomposites at 374% and the maximum relative resistance changes (ΔR/R0) of 20 and 200 at 0.9 and 7.5% strains, respectively, were recorded in the nanocomposites (3 wt.-% MWCNTs) within the estimated volume resistivity range. A cyclic strain experiment shows the most stable and reproducible ΔR/R0 values in the 2%–5% strain range. The electrical conductivity and piezoresistivity of the investigated nanocomposites in correlation with the mechanical properties and observed morphology make them applicable for low-strain deformation-sensing.
  • Item
    The effect of branched carbon nanotubes as reinforcing nano-filler in polymer nanocomposites
    (London : Elsevier, 2022) Thompson, S.M.; Talò, M.; Krause, Beate; Janke, A.; Lanzerotti, M.; Capps, J.; Lanzara, G.; Lacarbonara, W.
    This work discusses the mechanical and dissipative properties of nanocomposite materials made of a high-performance thermoplastic polymer (polybutylene terephthalate, PBT) integrated with branched carbon nanotubes (bCNTs) as nanofiller. The storage and loss moduli as well as the loss factor/damping ratio of the nanocomposites are experimentally characterized for increasing bCNT weight fractions (wt% bCNT) upon variations of the input cyclic strain amplitude and of the input frequency, respectively. The trends obtained for the nanocomposites mechanical properties indicate improvements both in storage and loss modulus by increasing the bCNT weight fraction from 0.5% to 2%. The striking differences between the damping capacities exhibited by CNT/polymer and bCNT/polymer nanocomposites are discussed to shed light onto the different underlined mechanics of the nanocomposites. Due to the stick–slip relative sliding motion of the polymer chains with respect to the straight CNTs, CNT/PBT nanocomposites are known to exhibit a peak in the damping vs. strain amplitude curves, past which, the damping capacity shows a monotonically increasing trend due to the conjectured sliding of the polymer crystals. On the other hand, we show for the first time that bCNT/PBT nanocomposites do not exhibit a peak in the damping capacity but rather a plateau after an initial drop at low strains. This behavior is attributed to the much reduced mobility of the branched CNTs and the lack of formation of crystalline structures around the bCNTs.
  • Item
    Polyethylene Glycol as Additive to Achieve N-Conductive Melt-Mixed Polymer/Carbon Nanotube Composites for Thermoelectric Application
    (Basel : MDPI, 2022) Krause, Beate; Pötschke, Petra
    The development of thermoelectric (TE) materials based on thermoplastic polymers and carbon nanotubes is a focus of current TE research activities. For a TE module, both p- and n-conductive composites are required, whereby the production of n-conductive materials is a particular challenge. The present study investigates whether adding polyethylene glycol (PEG) as n-dopant during the melt-mixing of the conductive composites based on polycarbonate, poly(ether ether ketone), or poly(butylene terephthalate) with singlewalled carbon nanotubes (0.5 to 2 wt%) is a possible solution. It was shown that for all three polymer types, a change in the sign of the Seebeck coefficient from positive to negative could be achieved when at least 1.5 wt% PEG was added. The most negative Seebeck coefficients were determined to be −30.1 µV/K (PC), −44.1 µV/K (PEEK), and −14.5 µV/K (PBT). The maximal power factors ranged between 0.0078 µW/m·K2 (PC), 0.035 µW/m·K2 (PEEK), and 0.0051 µW/m·K2 (PBT).
  • Item
    Thermoelectric Properties of N-Type Poly (Ether Ether Ketone)/Carbon Nanofiber Melt-Processed Composites
    (Basel : MDPI, 2022) Paleo, Antonio Jose; Krause, Beate; Soares, Delfim; Melle-Franco, Manuel; Muñoz, Enrique; Pötschke, Petra; Rocha, Ana Maria
    The thermoelectric properties, at temperatures from 30 °C to 100 °C, of melt-processed poly(ether ether ketone) (PEEK) composites prepared with 10 wt.% of carbon nanofibers (CNFs) are discussed in this work. At 30 °C, the PEEK/CNF composites show an electrical conductivity (σ) of ~27 S m−1 and a Seebeck coefficient (S) of −3.4 μV K−1, which means that their majority charge carriers are electrons. The origin of this negative Seebeck is deduced because of the impurities present in the as-received CNFs, which may cause sharply varying and localized states at approximately 0.086 eV above the Fermi energy level (EF) of CNFs. Moreover, the lower S, in absolute value, found in PEEK/CNF composites, when compared with the S of as-received CNFs (−5.3 μV K−1), is attributed to a slight electron withdrawing from the external layers of CNFs by the PEEK matrix. At temperatures from 30 °C to 100 °C, the σ (T) of PEEK/CNF composites, in contrast to the σ (T) of as-received CNFs, shows a negative temperature effect, understood through the 3D variable-range hopping (VRH) model, as a thermally activated hopping mechanism across a random network of potential wells. Moreover, their nonlinear S (T) follows the same behavior reported before for polypropylene composites melt-processed with similar CNFs at the same interval of temperatures.
  • Item
    Messanlage zur Untersuchung des Seebeck-Effektes in Polymermaterialien
    (Berlin : De Gruyter, 2020) Jenschke, Wolfgang; Ullrich, Mathias; Krause, Beate; Pötschke, Petra
    The thermoelectric effect named after the physicist Thomas Johann Seebeck has been investigated sufficiently well for all technically relevant metals and has been used for a long time, among other things, for temperature measurement by means of thermocouples. Less well known and researched is the Seebeck effect in polymer materials, which are gaining increasing influence in the sensor industry today. This article describes a measuring system designed specifically to study the Seebeck effect in polymeric samples with the aim of developing tailored polymers for sensory engineering applications using the Seebeck effect. The special requirement of the measuring system is the realization of constant accurate temperature sources.
  • Item
    Graphite modified epoxy-based adhesive for joining of aluminium and PP/graphite composites
    (New York, NY [u.a.] : Taylor & Francis, 2020) Rzeczkowski, P.; Pötschke, Petra; Fischer, M.; Kühnert, I.; Krause, Beate
    A graphite-modified adhesive was developed in order to simultaneously enhance the thermal conductivity and the strength of an adhesive joint. The thermal conductivity through the joint was investigated by using highly filled PP/graphite composite substrates, which were joined with an epoxy adhesive of different layer thicknesses. Similar measurements were carried out with a constant adhesive layer thickness, whilst applying an epoxy adhesive modified with expanded graphite (EG) (6, 10, and 20 wt%). By reducing the adhesive layer thickness or modifying the adhesive with conductive fillers, a significant increase of the thermal conductivity through the joint was achieved. The examination of the mechanical properties of the modified adhesives was carried out by tensile tests (adhesive only), lap-shear tests, and fracture energy tests (mode 1) with aluminium substrates. Modification of the adhesive with EG led to an increase of the tensile lap-shear strength and the adhesive fracture energy (mode 1) of the joint. In addition, burst pressure tests were performed to determine the strength of the joint in a complex component. The strength of the joint increased with the graphite content in the PP substrate and in the epoxy adhesive.