Search Results

Now showing 1 - 10 of 17
  • Item
    Temperature-dependent electric noise level in different iron-based superconductors
    (Milton Park : Taylor & Francis, 2014) Barone, C.; Pagano, S.; Bellingeri, E.; Ferdeghini, C.; Adamo, M.; Sarnelli, E.; Yokoyama, K.; Kurth, F.; Holzapfel, B; Iida, K.
    The magnetic flux penetration into the melt-textured Y-Ba-Cu-O high temperature superconducting bulk magnets were precisely evaluated during and after the pulsed field magnetization processes operated at 30 K. The bulk magnets were carefully fabricated by the cold seeding method with use of a single and a pair of seed crystals composed of the Nd-Ba-Cu-O thin films. These seed crystals were put on the top surfaces of the precursors to let the large grains grow during the heat treatments. We observed the flux penetrations which occurred in the lower applied-field regions at around 3.1 T for the samples bearing the twin seeds than those of the single-seeded crystals at around 3.8 T. This means that the magnetic fluxes are capable of invading into the twin-seeded samples more easily than the single-seeds. It suggests that the anisotropic grain growths of parallel and normal to the rows of seed crystals affects the variations of Jc values with different distributions of the pinning centers, results in the preferential paths for the invading magnetic fluxes.
  • Item
    Pulsed-field Invasion to HTS Bulk Magnets Grown from Two Seeds with Varied Seed-crystal Positions and Numbers
    (Amsterdam [u.a.] : Elsevier, 2014) Oka, T.; Yamada, Y.; Horiuchi, T.; Ogawa, J.; Fukui, S.; Sato, T.; Yokoyama, K.; Langer, M.
    The flux-invasion behavior into the melt-processed Y-Ba-Cu-O bulk magnets were precisely measured and analyzed during and after their pulsed-field magnetization processes operated at 30.6 K. The materials were fabricated as the bulk monoliths grown by adopting two seed-crystals, or shifting the seed-crystal positions from the centre of the sample surface, which exhibited the magnetically single-domain distributions. Although the performances of the trapped flux density after activations showed no obvious differences, the flux started invading into the sample bearing two seeds obviously at lower fields than those of normally-grown isotropic crystal. Since the flux penetration behavior were thus clearly different between the samples with the structure grown from two seeds and uniformly grown samples with a seed crystal, it is suggested that the structure results in an effective magnetizing method with less heating than those of conventional samples, which results in the higher performance of field trapping in the bulk magnets than usual.
  • Item
    Bicrystalline grain boundary junctions of Co-doped and P-doped Ba-122 thin films
    (Milton Park : Taylor & Francis, 2014) Schmidt, S.; Döring, S.; Schmidl, F.; Kurth, F.; Iida, K.; Holzapfel, B.; Kawaguchi, T.; Mori, Y.; Ikuta, H.; Seidel, P.
    We prepared GB junctions of Ba(Fe0.9Co0.1)2As2 thin films on bicrystalline [00 l]-tilt SrTiO3 substrates. The junctions show clear Josephson effects. Electrical characterization shows asymmetric I-V characteristics which can be described within the resistively shunted junction (RSJ) model. A large excess current is observed. Their formal ICRN product is 20.2 μV at 4.2 K, which is decreased to 6.5 μV when taking Iex into account. Fabrication methods to increase this value are discussed. Additionally, measurements on GB junctions of BaFe2(As0.66P0.34)2 thin films on LSAT bicrystalline substrates are shown. Their symmetric RSJ/flux flow-behavior exhibits a formal ICRN product of 45 μV, whereas the excess corrected value is ll μV.
  • Item
    Pulsed laser deposition of thick BaHfO3-doped YBa 2Cu307-δ films on highly alloyed textured Ni-W tapes
    (Bristol : Institute of Physics Publishing, 2014) Sieger, M.; Hänisch, J.; Iida, K.; Gaitzsch, U.; Rodig, C.; Schultz, L.; Holzapfel, B.; Hühne, R.
    YBa2Cu3O7-δ (YBCO) films with a thickness of up to 3 μm containing nano-sized BaHfO3 (BHO) have been grown on Y2O3/Y-stabilized ZrO2/CeO 2 buffered Ni-9at% W tapes by pulsed laser deposition (PLD). Structural characterization by means of X-ray diffraction confirmed that the YBCO layer grew epitaxial. A superconducting transition temperature T c of about 89 K with a transition width of 1 K was determined, decreasing with increasing BHO content. Critical current density in self-field and at 0.3 T increased with increasing dopant level.
  • Item
    Magnetic flux-trapping of anisotropic-grown Y-Ba-Cu-O bulk superconductors during and after pulsed-field magnetizing processes
    (Milton Park : Taylor & Francis, 2014) Oka, T.; Yamada, Y.; Horiuchi, T.; Ogawa, J.; Fukui, S.; Sato, T.; Yokoyama, K.; Langer, M.
    The magnetic flux penetration into the melt-textured Y-Ba-Cu-O high temperature superconducting bulk magnets were precisely evaluated during and after the pulsed field magnetization processes operated at 30 K. The bulk magnets were carefully fabricated by the cold seeding method with use of a single and a pair of seed crystals composed of the Nd-Ba-Cu-O thin films. These seed crystals were put on the top surfaces of the precursors to let the large grains grow during the heat treatments. We observed the flux penetrations which occurred in the lower applied-field regions at around 3.1 T for the samples bearing the twin seeds than those of the single-seeded crystals at around 3.8 T. This means that the magnetic fluxes are capable of invading into the twin-seeded samples more easily than the single-seeds. It suggests that the anisotropic grain growths of parallel and normal to the rows of seed crystals affects the variations of Jc values with different distributions of the pinning centers, results in the preferential paths for the invading magnetic fluxes.
  • Item
    Quasi-static and dynamic deformation behaviour of Zr-based bulk metallic glass
    (Milton Park : Taylor & Francis, 2013) Nekouie, V.; Kühn, U.; Roy, A.; Silberschmidt, V.
    Nano- and micro-indentation studies were carried out to characterise a plasticity mechanism through the evolution of localised shear bands that drive material's deformation at sub-micron length scale. Initial deformation of Zr-based bulk metallic glass (BMG) was investigated with nanoindentation tests using a spherical indenter. The indentation cycle reflects an elastic deformation with the yielding load of approx. 3 mN. For designed cycling indentation, hardening and softening phenomena were observed in nano- and micro-indentations, respectively. High-precision dynamic mechanical relaxation measurements were performed using a Dynamic Mechanical Analyzer (DMA), on decreasing frequency from 160 Hz to 0.1 Hz. A mechanical response of the BMG surface to a concentrated impact load was also studied. The obtained results indicated that the studied Zr-based BMG behaved as an elastic-perfectly plastic material at macroscale with discrete plasticity events at smaller length scales.
  • Item
    Measurements of Streams Agitated by Fluid Loaded SAW-devices Using a Volumetric 3-component Measurement Technique (V3V)
    (Amsterdam [u.a.] : Elsevier, 2015) Kiebert, Florian; König, Jörg; Kykal, Carsten; Schmidt, Hagen
    Utilizing surface acoustic waves (SAW) to induce tailored fluid motion via the acoustic streaming requires detailed knowledge about the acoustic bulk wave excitation. For the first time, the Defocus Digital Particle Image Velocimetry is used to measure the fluid motion originating from a fluid loaded SAW-device. With this flow measurement technique, the acoustic streaming-induced fluid motion can be observed volumetrically, which is attractive not only for application, but also for simulation in order to gain deeper insights regarding three-dimensional acoustic effects.
  • Item
    Investigation of the strain-sensitive superconducting transition of BaFe1.8Co0.2As2 thin films utilizing piezoelectric substrates
    (Milton Park : Taylor & Francis, 2014) Trommler, S.; Hänisch, J.; Iida, K.; Kurth, F.; Schultz, L.; Holzapfel, B.; Hühne, R.
    The preparation of biaxially textured BaFe1.8Co0.2As2 thin films has been optimized on MgO single crystals and transfered to piezoelectric (001) Pb(Mg1/3Nb2/3)0.72Ti0.28O3 substrates. By utilizing the inverse piezoelectric effect the lattice parameter of these substrates can be controlled applying an electric field, leading to a induction of biaxial strain into the superconducting layer. High electric fields were used to achieve a total strain of up to 0.05% at low temperatures. A sharpening of the resistive transition and a shift of about 0.6 K to higher temperatures was found at a compressive strain of 0.035%.
  • Item
    Three-Dimensional Imaging of Magnetic Domains with Neutron Grating Interferometry
    (Amsterdam [u.a.] : Elsevier, 2015) Manke, I.; Kardjilov, N.; Schäfer, R.; Hilger, A.; Grothausmann, R.; Strobl, M.; Dawson, M.; Grünzweig, Ch.; Tötzke, Ch.; David, Ch.; Kupsch, A.; Lange, A.; Hentschel, M.P.; Banhart, J.
    This paper gives a brief overview on3D imaging of magnetic domains with shearing grating neutron tomography. We investigated the three-dimensional distribution of magnetic domain walls in the bulk of a wedge-shaped FeSi single crystal. The width of the magnetic domains wasanalyzed at different locations within the crystal. Magnetic domains close to the tip of the wedge are much smaller than in the bulk. Furthermore, the three-dimensional shape of individual domains wasinvestigated. We discuss prospects and limitations of the applied measurement technique.
  • Item
    Determination of Bulk Magnetic Volume Properties by Neutron Dark-Field Imaging
    (Amsterdam [u.a.] : Elsevier, 2015) Grünzweig, Christian; Siebert, René; Betz, Benedikt; Rauscher, Peter; Schäfer, Rudolf; Lehmann, Eberhard
    For the production of high-class electrical steel grades a deeper understanding of the magnetic domain interaction with induced mechanical stresses is strongly required. This holds for non-oriented (NO) as well as grain-oriented (GO) steels. In the case of non-oriented steels the magnetic property degeneration after punching or laser cutting is essential for selecting correct obstructing material grades and designing efficient electrical machines. Until now these effects stay undiscovered due to the lack of adequate investigation methods that reveal local bulk information on processed laminations. Here we show how the use of a non-destructive testing method based on a neutron grating interferometry providing the dark-field image contrast delivers spatially-resolved transmission information about the local bulk domain arrangement and domain wall density. With the help of this technique it is possible to visualize magnetization processes within the NO laminations. Different representative manufacturing techniques are compared in terms of magnetic flux density deterioration such as punching, mechanically cutting by guillotine as well as laser fusion cutting using industrial high power laser beam sources. For GO steel laminations the method is applicable on the one hand to visualize the internal domain structure without being hindered by the coating layer. On the other hand, we can show the influence of the coating layer onto the underlying domain structure.