    Single-crystal neutron and X-ray diffraction study of garnet-type solid-state electrolyte Li6La3ZrTaO12: An in situ temperature-dependence investigation (2.5 ≤ T ≤ 873 K)
    (Oxford [u.a.] : Wiley-Blackwell, 2021) Redhammer, Günther J.; Meven, Martin; Ganschow, Steffen; Tippelt, Gerold; Rettenwander, Daniel
    Large single crystals of garnet-type Li6La3ZrTaO12 (LLZTO) were grown by the Czochralski method and analysed using neutron diffraction between 2.5 and 873 K in order to fully characterize the Li atom distribution, and possible Li ion mobility in this class of potential candidates for solid-state electrolyte battery material. LLZTO retains its cubic symmetry (space group Ia 3 d) over the complete temperature range. When compared to other sites, the octahedral sites behave as the most rigid unit and show the smallest increase in atomic displacement parameters and bond length. The La and Li sites show similar thermal expansion in their bond lengths with temperature, and the anisotropic and equivalent atomic displacement parameters exhibit a distinctly larger increase at temperatures above 400 K. Detailed inspection of nuclear densities at the Li1 site reveal a small but significant displacement from the 24d position to the typical 96h position, which cannot, however, be resolved from the single-crystal X-ray diffraction data. The site occupation of LiI ions on Li1 and Li2 sites remains constant, so there is no change in site occupation with temperature. © 2021 International Union of Crystallography. All rights reserved.
  • Item
    The natural critical current density limit for Li7La3Zr2O12 garnets
    (London [u.a.] : RSC, 2020) Flatscher, Florian; Philipp, Martin; Ganschow, Steffen; Wilkening, H. Martin R.; Rettenwander, Daniel
    Ceramic batteries equipped with Li-metal anodes are expected to double the energy density of conventional Li-ion batteries. Besides high energy densities, also high power is needed when batteries have to be developed for electric vehicles. Practically speaking, so-called critical current densities (CCD) higher than 3 mA cm-2 are needed to realize such systems. As yet, this value has, however, not been achieved for garnet-type Li7La3Zr2O12 (LLZO) being one of the most promising ceramic electrolytes. Most likely, CCD values are influenced by the area specific resistance (ASR) governing ionic transport across the Li|electrolyte interface. Here, single crystals of LLZO with adjusted ASR are used to quantify this relationship in a systematic manner. It turned out that CCD values exponentially decrease with increasing ASR. The highest obtained CCD value was as high as 280 µA cm-2. This value should be regarded as the room-temperature limit for LLZO when no external pressure is applied. Concluding, for polycrystalline samples either stack pressure or a significant increase of the interfacial area is needed to reach current densities equal or higher than the above-mentioned target value. This journal is © The Royal Society of Chemistry.
  • Item
    Investigating the electrochemical stability of Li7La3Zr2O12 solid electrolytes using field stress experiments
    (London [u.a.] : RSC, 2021) Smetaczek, Stefan; Pycha, Eva; Ring, Joseph; Siebenhofer, Matthäus; Ganschow, Steffen; Berendts, Stefan; Nenning, Andreas; Kubicek, Markus; Rettenwander, Daniel; Limbeck, Andreas; Fleig, Jürgen
    Cubic Li7La3Zr2O12 (LLZO) garnets are among the most promising solid electrolytes for solid-state batteries with the potential to exceed conventional battery concepts in terms of energy density and safety. The electrochemical stability of LLZO is crucial for its application, however, controversial reports in the literature show that it is still an unsettled matter. Here, we investigate the electrochemical stability of LLZO single crystals by applying electric field stress via macro- and microscopic ionically blocking Au electrodes in ambient air. Induced material changes are subsequently probed using various locally resolved analysis techniques, including microelectrode electrochemical impedance spectroscopy (EIS), laser induced breakdown spectroscopy (LIBS), laser ablation-inductively coupled plasma-mass spectrometry (LA-ICP-MS), and microfocus X-ray diffraction (XRD). Our experiments indicate that LLZO decomposes at 4.1–4.3 V vs. Li+/Li, leading to the formation of Li-poor phases like La2Zr2O7 beneath the positively polarized electrode. The reaction is still on-going even after several days of polarization, indicating that no blocking interfacial layer is formed. The decomposition can be observed at elevated as well as room temperature and suggests that LLZO is truly not compatible with high voltage cathode materials.
  • Item
    Melt Growth and Physical Properties of Bulk LaInO3 Single Crystals
    (Weinheim : Wiley-VCH, 2021) Galazka, Zbigniew; Irmscher, Klaus; Ganschow, Steffen; Zupancic, Martina; Aggoune, Wahib; Draxl, Claudia; Albrecht, Martin; Klimm, Detlef; Kwasniewski, Albert; Schulz, Tobias; Pietsch, Mike; Dittmar, Andrea; Grueneberg, Raimund; Juda, Uta; Schewski, Robert; Bergmann, Sabine; Cho, Hyeongmin; Char, Kookrin; Schroeder, Thomas; Bickermann, Matthias
    Large bulk LaInO3 single crystals are grown from the melt contained within iridium crucibles by the vertical gradient freeze (VGF) method. The obtained crystals are undoped or intentionally doped with Ba or Ce, and enabled wafer fabrication of size 10 × 10 mm2. High melting point of LaInO3 (≈1880 °C) and thermal instability at high temperatures require specific conditions for bulk crystal growth. The crystals do not undergo any phase transition up to 1300 °C, above which a noticeable thermal decomposition takes place. The good structural quality of the crystals makes them suitable for epitaxy. The onset of strong optical absorption shows orientation-dependent behavior due to the orthorhombic symmetry of the LaInO3 crystals. Assuming direct transitions, optical bandgaps of 4.35 and 4.39 eV are obtained for polarizations along the [010] and the [100], [001] crystallographic directions, respectively. There is an additional weak absorption in the range between 2.8 and 4 eV due to oxygen vacancies. Density-functional-theory calculations support the interpretation of the optical absorption data. Cathodoluminescence spectra show a broad, structured emission band peaking at ≈2.2 eV. All bulk crystals are electrically insulating. The relative static dielectric constant is determined at a value of 24.6 along the [001] direction.
  • Item
    Bulk single crystals and physical properties of β-(AlxGa1-x)2O3(x = 0-0.35) grown by the Czochralski method
    (Melville, NY : American Inst. of Physics, 2023) Galazka, Zbigniew; Fiedler, Andreas; Popp, Andreas; Ganschow, Steffen; Kwasniewski, Albert; Seyidov, Palvan; Pietsch, Mike; Dittmar, Andrea; Anooz, Saud Bin; Irmscher, Klaus; Suendermann, Manuela; Klimm, Detlef; Chou, Ta-Shun; Rehm, Jana; Schroeder, Thomas; Bickermann, Matthias
    We have systematically studied the growth, by the Czochralski method, and basic physical properties of a 2 cm and 2 in. diameter bulk β-(AlxGa1-x)2O3 single crystal with [Al] = 0-35 mol. % in the melt in 5 mol. % steps. The segregation coefficient of Al in the Ga2O3 melt of 1.1-1.2 results in a higher Al content in the crystals than in the melt. The crystals were also co-doped with Si or Mg. [Al] = 30 mol. % in the melt (33-36 mol. % in the crystals) seems to be a limit for obtaining bulk single crystals of high structural quality suitable for homoepitaxy. The crystals were either semiconducting (no intentional co-dopants with [Al] = 0-30 mol. % and Si-doped with [Al] = 15-20 mol. %), degenerately semiconducting (Si-doped with [Al] ≤ 15 mol. %), or semi-insulating ([Al] ≥ 25 mol. % and/or Mg-doped). The full width at half maximum of the rocking curve was 30-50 arcsec. The crystals showed a linear but anisotropic decrease in all lattice constants and a linear increase in the optical bandgap (5.6 eV for [Al] = 30 mol. %). The room temperature electron mobility at similar free electron concentrations gradually decreases with [Al], presumably due to enhanced scattering at phonons as the result of a larger lattice distortion. In Si co-doped crystals, the scattering is enhanced by ionized impurities. Measured electron mobilities and bandgaps enabled to estimate the Baliga figure of merit for electronic devices.
  • Item
    Spectroscopy and 2.1 µm laser operation of Czochralski-grown Tm3+:YScO3 crystals
    (Washington, DC : Soc., 2022) Suzuki, Anna; Kalusniak, Sascha; Tanaka, Hiroki; Brützam, Mario; Ganschow, Steffen; Tokurakawa, Masaki; Kränkel, Christian
    We report on growth, temperature-dependent spectroscopy, and laser experiments of Tm3+-doped YScO3 mixed sesquioxide crystals. For the first time, cm3-scale laser quality Tm3+:YScO3 crystals with 2.2 at.% and 3.1 at.% doping levels were grown by the Czochralski method from iridium crucibles. We reveal that the structural disorder in the mixed crystals allows for broad and smooth spectral features even at cryogenic temperatures. We obtained the first continuous wave laser operation in this material at wavelengths around 2100 nm using a laser diode emitting at 780 nm as a pump source. A maximum slope efficiency of 45% was achieved using a Tm3 + (3.1 at.%):YScO3 crystal. Our findings demonstrate the high potential of Tm3+-doped mixed sesquioxides for efficient ultrafast pulse generation in the 2.1 µm range.