Search Results

Now showing 1 - 2 of 2
  • Item
    Electrically conductive and piezoresistive polymer nanocomposites using multiwalled carbon nanotubes in a flexible copolyester: Spectroscopic, morphological, mechanical and electrical properties
    (Amsterdam [u.a.] : Elsevier, 2022) Dhakal, Kedar Nath; Khanal, Santosh; Krause, Beate; Lach, Ralf; Grellmann, Wolfgang; Le, Hai Hong; Das, Amit; Wießner, Sven; Heinrich, Gert; Pionteck, Jürgen; Adhikari, Rameshwar
    Nanocomposites of multiwalled carbon nanotubes (MWCNTs) with poly(butylene adipate-co-terephthalate) (PBAT), a flexible aromatic–aliphatic copolyester, were prepared by melt mixing followed by compression moulding to investigate their spectroscopic, morphological, mechanical and electrical properties. A comparison of the Fourier transform infrared (FTIR) spectra of the neat polymer matrix and the composites showed no difference, implying a physical mixing of the matrix and the filler. A morphological investigation revealed the formation of a continuous and interconnected MWCNT network embedded in the polymer matrix with partial agglomeration. Increasing Martens hardness and indentation modulus and decreasing maximum indentation depth with increasing filler concentration demonstrated the reinforcement of the polymer by the MWCNTs. A volume resistivity of 4.6 × 105 Ω cm of the materials was achieved by the incorporation of only 1 wt.-% of the MWCNTs, which confirmed a quite low percolation threshold (below 1 wt.-%) of the nanocomposites. The electrical volume resistivity of the flexible nanocomposites was achieved up to 1.6 × 102 Ω cm, depending on the filler content. The elongation at the break of the nanocomposites at 374% and the maximum relative resistance changes (ΔR/R0) of 20 and 200 at 0.9 and 7.5% strains, respectively, were recorded in the nanocomposites (3 wt.-% MWCNTs) within the estimated volume resistivity range. A cyclic strain experiment shows the most stable and reproducible ΔR/R0 values in the 2%–5% strain range. The electrical conductivity and piezoresistivity of the investigated nanocomposites in correlation with the mechanical properties and observed morphology make them applicable for low-strain deformation-sensing.
  • Item
    Thermoelectric Performance of Polypropylene/Carbon Nanotube/Ionic Liquid Composites and Its Dependence on Electron Beam Irradiation
    (Basel : MDPI, 2022-1-11) Voigt, Oliver; Krause, Beate; Pötschke, Petra; Müller, Michael T.; Wießner, Sven
    The thermoelectric behavior of polypropylene (PP) based nanocomposites containing single walled carbon nanotubes (SWCNTs) and five kinds of ionic liquids (Ils) dependent on composite composition and electron beam irradiation (EB) was studied. Therefore, several samples were melt-mixed in a micro compounder, while five Ils with sufficiently different anions and/or cations were incorporated into the PP/SWCNT composites followed by an EB treatment for selected composites. Extensive investigations were carried out considering the electrical, thermal, mechanical, rheological, morphological and, most significantly, thermoelectric properties. It was found that it is possible to prepare n-type melt-mixed polymer composites from p-type commercial SWCNTs with relatively high Seebeck coefficients when adding four of the selected Ils. The highest Seebeck coefficients achieved in this study were +49.3 µV/K (PP/2 wt.% SWCNT) for p-type composites and −27.6 µV/K (PP/2 wt.% SWCNT/4 wt.% IL type AMIM Cl) for n-type composites. Generally, the type of IL is decisive whether p-or n-type thermoelectric behavior is achieved. After IL addition higher volume conductivity could be reached. Electron beam treatment of PP/SWCNT leads to increased values of the Seebeck coefficient, whereas the EB treated sample with IL (AMIM Cl) shows a less negative Seebeck coefficient value.