  • Item
    2 MW peak power generation in fluorine co-doped Yb fiber prepared by powder-sinter technology
    (Washington, DC : Soc., 2020) Leich, Martin; Kalide, André; Eschrich, Tina; Lorenz, Adrian; Lorenz, Martin; Wondraczek, Katrin; Schönfeld, Dörte; Langner, Andreas; Schötz, Gerhard; Jäger, Matthias
    We report on the first, to the best of our knowledge, implementation of a fluorine co-doped large-mode-area REPUSIL fiber for high peak power amplification in an ultrashort-pulse master oscillator power amplifier. The core material of the investigated step-index fiber with high Yb-doping level, 52 µm core and high core-to-clad ratio of 1:4.2 was fabricated by means of the REPUSIL powder-sinter technology. The core numerical aperture was adjusted by fluorine codoping to 0.088. For achieving high beam quality and for ensuring a monolithic seed path, the LMA fiber is locally tapered. We demonstrate an Yb fiber amplifier with near-diffraction-limited beam quality of M2 = 1.3, which remains constant up to a peak power of 2 MW. This is a record for a tapered single core fiber. © 2020 Optical Society of America
  • Item
    Taming Ultrafast Laser Filaments for Optimized Semiconductor–Metal Welding
    (Weinheim : Wiley VCH, 2021) Chambonneau, Maxime; Li, Qingfeng; Fedorov, Vladimir Yu.; Blothe, Markus; Schaarschmidt, Kay; Lorenz, Martin; Tzortzakis, Stelios; Nolte, Stefan
    Ultrafast laser welding is a fast, clean, and contactless technique for joining a broad range of materials. Nevertheless, this technique cannot be applied for bonding semiconductors and metals. By investigating the nonlinear propagation of picosecond laser pulses in silicon, it is elucidated how the evolution of filaments during propagation prevents the energy deposition at the semiconductor–metal interface. While the restrictions imposed by nonlinear propagation effects in semiconductors usually inhibit countless applications, the possibility to perform semiconductor–metal ultrafast laser welding is demonstrated. This technique relies on the determination and the precompensation of the nonlinear focal shift for relocating filaments and thus optimizing the energy deposition at the interface between the materials. The resulting welds show remarkable shear joining strengths (up to 2.2 MPa) compatible with applications in microelectronics. Material analyses shed light on the physical mechanisms involved during the interaction. © 2020 The Authors. Laser & Photonics Reviews published by Wiley-VCH GmbH
  • Item
    Yb-doped large mode area fiber for beam quality improvement using local adiabatic tapers with reduced dopant diffusion
    (Washington D.C. : Optical Society of America, 2018) Zhu, Yuan; Leich, Martin; Lorenz, Martin; Eschrich, Tina; Aichele, Claudia; Kobelke, Jens; Bartelt, Hartmut; Jäger, Matthias
    A newly designed all-solid step-index Yb-doped aluminosilicate large mode area fiber for achieving high peak power at near diffraction limited beam quality with local adiabatic tapering is presented. The 45µm diameter fiber core and pump cladding consist of active/passively doped aluminosilicate glass produced by powder sinter technology (REPUSIL). A deliberate combination of innovative cladding and core materials was aspired to achieve low processing temperature reducing dopant diffusion during fiber fabrication, tapering and splicing. By developing a short adiabatic taper, robust seed coupling is achieved by using this Yb-doped LMA fiber as final stage of a nanosecond fiber Master Oscillator Power Amplifier (MOPA) system while maintaining near diffraction limited beam quality by preferential excitation of the fundamental mode. After application of a fiber-based endcap, the peak power could be scaled up to 375 kW with high beam quality and a measured M2 value of 1.3~1.7.A newly designed all-solid step-index Yb-doped aluminosilicate large mode area fiber for achieving high peak power at near diffraction limited beam quality with local adiabatic tapering is presented. The 45µm diameter fiber core and pump cladding consist of active/passively doped aluminosilicate glass produced by powder sinter technology (REPUSIL). A deliberate combination of innovative cladding and core materials was aspired to achieve low processing temperature reducing dopant diffusion during fiber fabrication, tapering and splicing. By developing a short adiabatic taper, robust seed coupling is achieved by using this Yb-doped LMA fiber as final stage of a nanosecond fiber Master Oscillator Power Amplifier (MOPA) system while maintaining near diffraction limited beam quality by preferential excitation of the fundamental mode. After application of a fiber-based endcap, the peak power could be scaled up to 375 kW with high beam quality and a measured M2 value of 1.3~1.7.