    The Localization Behavior of Different CNTs in PC/SAN Blends Containing a Reactive Component
    (Basel : MDPI, 2021-3-1) Gültner, Marén; Boldt, Regine; Formanek, Petr; Fischer, Dieter; Simon, Frank; Pötschke, Petra
    Co-continuous blend systems of polycarbonate (PC), poly(styrene-co-acrylonitrile) (SAN), commercial non-functionalized multi-walled carbon nanotubes (MWCNTs) or various types of commercial and laboratory functionalized single-walled carbon nanotubes (SWCNTs), and a reactive component (RC, N-phenylmaleimide styrene maleic anhydride copolymer) were melt compounded in one step in a microcompounder. The blend system is immiscible, while the RC is miscible with SAN and contains maleic anhydride groups that have the potential to reactively couple with functional groups on the surface of the nanotubes. The influence of the RC on the localization of MWCNTs and SWCNTs (0.5 wt.%) was investigated by transmission electron microscopy (TEM) and energy-filtered TEM. In PC/SAN blends without RC, MWCNTs are localized in the PC component. In contrast, in PC/SAN-RC, the MWCNTs localize in the SAN-RC component, depending on the RC concentration. By adjusting the MWCNT/RC ratio, the localization of the MWCNTs can be tuned. The SWCNTs behave differently compared to the MWCNTs in PC/SAN-RC blends and their localization occurs either only in the PC or in both blend components, depending on the type of the SWCNTs. CNT defect concentration and surface functionalities seem to be responsible for the localization differences.
  • Item
    Correlation of carbon nanotube dispersability in aqueous surfactant solutions and polymers
    (New York, NY [u.a.] : Pergamon Press, 2009) Krause, Beate; Petzold, Gudrun; Pegel, Sven; Pötschke, Petra
    In order to assess the dispersability of carbon nanotube materials, tubes produced under different synthesis conditions were dispersed in aqueous surfactant solutions and the sedimentation behaviour under centrifugation forces was investigated using a LUMiFuge stability analyzer. The electrical percolation threshold of the nanotubes after melt mixing in polyamide 6.6 was determined and the state of dispersion was studied. As a general tendency, the nanotubes having better aqueous dispersion stability showed lower electrical percolation threshold and better nanotube dispersion in the composites. This indicates that the investigation of the stability of aqueous dispersions is also able to give information about the nanotubes inherent dispersability in polymer melts, both strongly influenced by the entanglement and agglomerate structure of the tubes within the as-produced nanotube materials. The shape of the nanotubes in the aqueous dispersions was assessed using a SYSMEX flow particle image analyzer and found to correspond to the shape observed from cryofractured surfaces of the polymer composites. © 2008 Elsevier Ltd. All rights reserved.
  • Item
    Electrically Conductive Polyetheretherketone Nanocomposite Filaments: From Production to Fused Deposition Modeling
    (Basel : MDPI, 2018-8-18) Gonçalves, Jordana; Lima, Patrícia; Krause, Beate; Pötschke, Petra; Lafont, Ugo; Gomes, José R.; Abreu, Cristiano S.; Paiva, Maria C.; Covas, José A.
    The present work reports the production and characterization of polyetheretherketone (PEEK) nanocomposite filaments incorporating carbon nanotubes (CNT) and graphite nanoplates (GnP), electrically conductive and suitable for fused deposition modeling (FDM) processing. The nanocomposites were manufactured by melt mixing and those presenting electrical conductivity near 10 S/m were selected for the production of filaments for FDM. The extruded filaments were characterized for mechanical and thermal conductivity, polymer crystallinity, thermal relaxation, nanoparticle dispersion, thermoelectric effect, and coefficient of friction. They presented electrical conductivity in the range of 1.5 to 13.1 S/m, as well as good mechanical performance and higher thermal conductivity compared to PEEK. The addition of GnP improved the composites' melt processability, maintained the electrical conductivity at target level, and reduced the coefficient of friction by up to 60%. Finally, three-dimensional (3D) printed test specimens were produced, showing a Young's modulus and ultimate tensile strength comparable to those of the filaments, but a lower strain at break and electrical conductivity. This was attributed to the presence of large voids in the part, revealing the need for 3D printing parameter optimization. Finally, filament production was up-scaled to kilogram scale maintaining the properties of the research-scale filaments.