    Cellulose-carbon nanotube composite aerogels as novel thermoelectric materials
    (Amsterdam [u.a.] : Elsevier, 2018) Gnanaseelan, Minoj; Chen, Yian; Luo, Jinji; Krause, Beate; Pionteck, Jürgen; Pötschke, Petra; Qu, Haisong
    Thermoelectric materials based on cellulose/carbon nanotube (CNT) nanocomposites have been developed by a facile approach and the effects of amount (2–10 wt%) and types of CNTs (single-walled carbon nanotubes (SWCNTs) and multi-walled carbon nanotubes (MWCNTs)) on the morphology (films and aerogels) and the thermoelectric properties of the nanocomposites have been investigated. Composite films based on SWCNTs showed significantly higher electrical conductivity (5 S/cm at 10 wt%) and Seebeck coefficient (47.2 μV/K at 10 wt%) compared to those based on MWCNTs (0.9 S/cm and 11 μV/K, respectively). Lyophilization, leading to development of aerogels with sub-micron sized pores, decreased the electrical conductivity for both types by one order of magnitude, but did not affect the Seebeck coefficient of MWCNT based nanocomposites. For SWCNT containing aerogels, higher Seebeck coefficients than for films were measured at 3 and 4 wt% but significantly lower values at higher loadings. CNT addition increased the thermal conductivity from 0.06 to 0.12 W/(m∙K) in the films, whereas the lyophilization significantly reduced it towards values between 0.01 and 0.09 W/(m∙K) for the aerogels. The maximum Seebeck coefficient, power factor, and ZT observed in this study are 49 μV/K for aerogels with 3 wt% SWCNTs, 1.1 μW/(m∙K2) for composite films with 10 wt% SWCNTs, and 7.4 × 10−4 for films with 8 wt% SWCNTs, respectively.
  • Item
    Nanocomposites with p-and n-type conductivity controlled by type and content of nanotubes in thermosets for thermoelectric applications
    (Basel : MDPI, 2020) Kröning, Katharina; Krause, Beate; Pötschke, Petra; Fiedler, Bodo
    In this work, composites based on epoxy resin and various carbon nanotubes (CNTs) were studied regarding their thermoelectric properties. The epoxy composites were prepared by infiltration of preformed CNT buckypapers. The influence of different types of CNTs on the Seebeck coefficient was investigated, namely lab-made and commercially available multi walled carbon nanotubes (MWCNTs), lab-made nitrogen doped MWCNTs (N-MWCNT) and commercially available single walled carbon nanotubes (SWCNTs). It was found that only by varying the lab-made MWCNT content could both n-and p-type composites be produced with Seebeck coefficients between -9.5 and 3.1 µV/K. The incorporation of N-MWCNTs resulted in negative Seebeck coefficients of -11.4 to -17.4 µV/K. Thus, the Seebeck coefficient of pure SWCNT changed from 37.4 to -25.5 µV/K in the epoxy/1 wt. % SWCNT composite. A possible explanation for the shift in the Seebeck coefficient is the change of the CNTs Fermi level depending on the number of epoxy molecules on the CNT surface. © 2020 by the authors. Licensee MDPI, Basel, Switzerland.
  • Item
    Thermoelectric Properties of N-Type Poly (Ether Ether Ketone)/Carbon Nanofiber Melt-Processed Composites
    (Basel : MDPI, 2022) Paleo, Antonio Jose; Krause, Beate; Soares, Delfim; Melle-Franco, Manuel; Muñoz, Enrique; Pötschke, Petra; Rocha, Ana Maria
    The thermoelectric properties, at temperatures from 30 °C to 100 °C, of melt-processed poly(ether ether ketone) (PEEK) composites prepared with 10 wt.% of carbon nanofibers (CNFs) are discussed in this work. At 30 °C, the PEEK/CNF composites show an electrical conductivity (σ) of ~27 S m−1 and a Seebeck coefficient (S) of −3.4 μV K−1, which means that their majority charge carriers are electrons. The origin of this negative Seebeck is deduced because of the impurities present in the as-received CNFs, which may cause sharply varying and localized states at approximately 0.086 eV above the Fermi energy level (EF) of CNFs. Moreover, the lower S, in absolute value, found in PEEK/CNF composites, when compared with the S of as-received CNFs (−5.3 μV K−1), is attributed to a slight electron withdrawing from the external layers of CNFs by the PEEK matrix. At temperatures from 30 °C to 100 °C, the σ (T) of PEEK/CNF composites, in contrast to the σ (T) of as-received CNFs, shows a negative temperature effect, understood through the 3D variable-range hopping (VRH) model, as a thermally activated hopping mechanism across a random network of potential wells. Moreover, their nonlinear S (T) follows the same behavior reported before for polypropylene composites melt-processed with similar CNFs at the same interval of temperatures.
  • Item
    Messanlage zur Untersuchung des Seebeck-Effektes in Polymermaterialien
    (Berlin : De Gruyter, 2020) Jenschke, Wolfgang; Ullrich, Mathias; Krause, Beate; Pötschke, Petra
    The thermoelectric effect named after the physicist Thomas Johann Seebeck has been investigated sufficiently well for all technically relevant metals and has been used for a long time, among other things, for temperature measurement by means of thermocouples. Less well known and researched is the Seebeck effect in polymer materials, which are gaining increasing influence in the sensor industry today. This article describes a measuring system designed specifically to study the Seebeck effect in polymeric samples with the aim of developing tailored polymers for sensory engineering applications using the Seebeck effect. The special requirement of the measuring system is the realization of constant accurate temperature sources.