  • Item
    783 nm wavelength stabilized DBR tapered diode lasers with a 7 W output power
    (Washington, DC : The Optical Society, 2021) Sumpf, Bernd; Theurer, Lara Sophie; Maiwald, Martin; Müller, André; Maaßdorf, André; Fricke, Jörg; Ressel, Peter; Tränkle, Günther
    Wavelength stabilized distributed Bragg reflector (DBR) tapered diode lasers at 783 nm will be presented. The devices are based on GaAsP single quantum wells embedded in a large optical cavity leading to a vertical far field angle of about 29◦ (full width at half maximum). The 3-inch (7.62 cm) wafers are grown using metalorganic vapor phase epitaxy. In a full wafer process, 4 mm long DBR tapered lasers are manufactured. The devices consist of a 500 µm long 10th order surface DBR grating that acts as rear side mirror. After that, a 1 mm long ridge waveguide section is realized for lateral confinement, which is connected to a 2.5 mm long flared section having a full taper angle of 6◦. At an injection current of 8 A, a maximum output power of about 7 W is measured. At output powers up to 6 W, the measured emission width limited by the resolution of the spectrometer is smaller than 19 pm. Measured at 1/e2 level at this output power, the lateral beam waist width is 11.5 µm, the lateral far field angle 12.5◦, and the lateral beam parameter M2 2.5. The respective parameters measured using the second moments are 31 µm, 15.2◦, and 8.3. 70% of the emitted power is originated from the central lobe. © 2021 Optical Society of America
  • Item
    Stability of ZnSe-Passivated Laser Facets Cleaved in Air and in Ultra-High Vacuum
    (New York, NY : IEEE, 2022) Boschker, Jos E.; Spengler, Uwe; Ressel, Peter; Schmidbauer, Martin; Mogilatenko, Anna; Knigge, Andrea
    Catastrophic optical mirror damage (COMD) is one of the main failure mechanisms limiting the reliability of GaAs based laser diodes. Here, we compare the facet stability of ZnSe-passivated ridge-waveguide lasers (RWLs) that are cleaved in air and subsequently cleaned using atomic hydrogen with RWLs that are cleaved in ultra-high vacuum. RWLs cleaved in ultra-high vacuum show a superior performance and reach power densities up to 58 MW/cm 2 under extended continuous wave operation at 1064 nm. This is attributed to the reduction of defects at the interface between ZnSe and the cleaved facet as evidenced by transmission electron microscopy and X-ray diffraction.