    Synthesis of Modified Poly(vinyl Alcohol)s and Their Degradation Using an Enzymatic Cascade
    (Weinheim : Wiley-VCH, 2023) von Haugwitz, Gerlis; Donnelly, Kian; Di Filippo, Mara; Breite, Daniel; Phippard, Max; Schulze, Agnes; Wei, Ren; Baumann, Marcus; Bornscheuer, Uwe T.
    Poly(vinyl alcohol) (PVA) is a water-soluble synthetic vinyl polymer with remarkable physical properties including thermostability and viscosity. Its biodegradability, however, is low even though a large amount of PVA is released into the environment. Established physical-chemical degradation methods for PVA have several disadvantages such as high price, low efficiency, and secondary pollution. Biodegradation of PVA by microorganisms is slow and frequently involves pyrroloquinoline quinone (PQQ)-dependent enzymes, making it expensive due to the costly cofactor and hence unattractive for industrial applications. In this study, we present a modified PVA film with improved properties as well as a PQQ-independent novel enzymatic cascade for the degradation of modified and unmodified PVA. The cascade consists of four steps catalyzed by three enzymes with in situ cofactor recycling technology making this cascade suitable for industrial applications.
  • Item
    Biocatalytic Degradation Efficiency of Postconsumer Polyethylene Terephthalate Packaging Determined by Their Polymer Microstructures
    (Weinheim : Wiley-VCH, 2019) Wei, Ren; Breite, Daniel; Song, Chen; Gräsing, Daniel; Ploss, Tina; Hille, Patrick; Schwerdtfeger, Ruth; Matysik, Jörg; Schulze, Agnes; Zimmermann, Wolfgang
    Polyethylene terephthalate (PET) is the most important mass-produced thermoplastic polyester used as a packaging material. Recently, thermophilic polyester hydrolases such as TfCut2 from Thermobifida fusca have emerged as promising biocatalysts for an eco-friendly PET recycling process. In this study, postconsumer PET food packaging containers are treated with TfCut2 and show weight losses of more than 50% after 96 h of incubation at 70 °C. Differential scanning calorimetry analysis indicates that the high linear degradation rates observed in the first 72 h of incubation is due to the high hydrolysis susceptibility of the mobile amorphous fraction (MAF) of PET. The physical aging process of PET occurring at 70 °C is shown to gradually convert MAF to polymer microstructures with limited accessibility to enzymatic hydrolysis. Analysis of the chain-length distribution of degraded PET by nuclear magnetic resonance spectroscopy reveals that MAF is rapidly hydrolyzed via a combinatorial exo- and endo-type degradation mechanism whereas the remaining PET microstructures are slowly degraded only by endo-type chain scission causing no detectable weight loss. Hence, efficient thermostable biocatalysts are required to overcome the competitive physical aging process for the complete degradation of postconsumer PET materials close to the glass transition temperature of PET.
  • Item
    Membrane Functionalization in Pilot Scale: Roll‐to‐Roll Electron Beam System with Inline Contact Angle Determination
    (Weinheim : Wiley-VCH, 2021) Schulze, Agnes; Drößler, Lutz; Weiß, Steffen; Went, Marco; Abdul Latif, Amira; Breite, Daniel; Fischer, Kristina
    To increase the permeation performance and antifouling properties of polymer membranes, a one-step reaction using electron irradiation was developed. This process combines the surface activation of the membrane polymer and the simultaneous permanent immobilization of hydrophilic molecules. This technology can be applied to various polymers, flat sheet/hollow fiber membranes and all pore ranges. The roll-to-roll system developed for this enables all process steps including inline analysis for quality control of the membrane surface in a continuously operated system. © 2021 The Authors. Chemie Ingenieur Technik published by Wiley-VCH GmbH