    Statistical Analysis of Mechanical Stressing in Short Fiber Reinforced Composites by Means of Statistical and Representative Volume Elements
    (Basel : MDPI, 2021) Breuer, Kevin; Spickenheuer, Axel; Stommel, Markus
    Analyzing representative volume elements with the finite element method is one method to calculate the local stress at the microscale of short fiber reinforced plastics. It can be shown with Monte-Carlo simulations that the stress distribution depends on the local arrangement of the fibers and is therefore unique for each fiber constellation. In this contribution the stress distribution and the effective composite properties are examined as a function of the considered volume of the representative volume elements. Moreover, the influence of locally varying fiber volume fraction is examined, using statistical volume elements. The results show that the average stress probability distribution is independent of the number of fibers and independent of local fluctuation of the fiber volume fraction. Furthermore, it is derived from the stress distributions that the statistical deviation of the effective composite properties should not be neglected in the case of injection molded components. A finite element analysis indicates that the macroscopic stresses and strains on component level are significantly influenced by local, statistical fluctuation of the composite properties.
  • Item
    Characterisation and Modelling of Moisture Gradients in Polyamide 6
    (Basel : MDPI, 2021) Sambale, Anna Katharina; Maisl, Michael; Herrmann, Hans-Georg; Stommel, Markus
    Polyamide 6 (PA6) is able to absorb water from the surrounding air and bond to it by forming hydrogen bonds between the carbonamide groups of its molecular chains. Diffusion processes cause locally different water concentrations in the (component) cross-section during the sorption process, resulting in locally different mechanical properties due to the water-induced plasticisation effect. However, the water content of PA6 is usually specified as an integral value, so no information about a local water distribution within a component is provided. This paper shows a method to characterise moisture distributions within PA6 samples using low-energy computer tomography (CT) techniques and comparing the reconstructed results with a developed finite elements (FE) modelling method based on Fick’s diffusion laws with concentration-dependent diffusion coefficients. For this purpose, the ageing of the samples at two different water bath temperatures as well as at different integral water contents are considered. The results obtained by CT reconstruction and FE modelling are in very good agreement, so that the concentration distributions by water sorption of PA6 calculated by FEM can be regarded as validated.
  • Item
    Characterisation and FE Modelling of the Sorption and Swelling Behaviour of Polyamide 6 in Water
    (Basel : MDPI, 2021) Sambale, Anna Katharina; Stanko, Michael; Emde, Jessica; Stommel, Markus
    Polyamide 6 (PA6) is known to absorb water from its environment due to its chemical structure. This water absorption leads to a change in the mechanical properties as well as an increase in volume (swelling) of the polyamide. In the present work, the sorption and swelling behaviour of polyamide 6 in different conditioning environments was experimentally investigated on different part geometries to develop a finite element (FE) method on the basis of the measured data that numerically calculates the sorption and swelling behaviour. The developed method includes two analyses using the Abaqus software. Both the concentration-dependent implementation of the simulation parameters and the calculation of swelling-induced stresses are performed. This enables the modelling of the sorption curves until maximum saturation is reached and the simulation of the characteristic S-shaped swelling curves. Therefore, the developed methodology represents an efficient method for predicting the sorption and swelling behaviour of polyamide 6 parts during conditioning in a water bath. The determined properties provide the basis for the development of an FE-based simulation environment to take moisture absorption into account during the part design. This enables the calculation of moisture-induced swelling processes and the resulting initial stresses in a given part.
  • Item
    Modelling and Experimental Investigation of Hexagonal Nacre-Like Structure Stiffness
    (Basel : MDPI, 2020) Rouhana, Rami; Stommel, Markus
    A highly ordered, hexagonal, nacre-like composite stiffness is investigated using experiments, simulations, and analytical models. Polystyrene and polyurethane are selected as materials for the manufactured specimens using laser cutting and hand lamination. A simulation geometry is made by digital microscope measurements of the specimens, and a simulation is conducted using material data based on component material characterization. Available analytical models are compared to the experimental results, and a more accurate model is derived specifically for highly ordered hexagonal tablets with relatively large in-plane gaps. The influence of hexagonal width, cut width, and interface thickness are analyzed using the hexagonal nacre-like composite stiffness model. The proposed analytical model converges within 1% with the simulation and experimental results
  • Item
    Correlation between Processing Parameters, Morphology, and Properties of Injection-Molded Polylactid Acid (PLA) Specimens at Different Length Scales
    (Basel : MDPI, 2023) Meinig, Laura; Boldt, Regine; Spoerer, Yvonne; Kuehnert, Ines; Stommel, Markus
    Polylactic acid (PLA) is one of the most promising bioplastic representatives that finds application in many different areas, e.g., as single-use products in the packaging industry, in the form of mulch film for agriculture, or in medical devices. For the development of new areas, especially in terms of long-term applications and the production of recyclable products, the material properties controlled by processing must be known. The state of the art is investigations at the global scale (integral values) without consideration of local structure inhomogeneities and their influence on the material properties. In this work, morphological, thermal, and mechanical properties of injection-molded PLA tensile bars are investigated at different length scales (global and local) as a function of processing parameters. In addition to the processing parameters, such as melt temperature, mold temperature, and cooling time in the mold, the influence of the D-isomer content on the crystallization behavior and the resulting material properties are investigated. The material was found to form crystalline structures only when cooled in a mold tempered above Tg. In addition, PLA with a lower content of D-isomer was found to have a higher degree of crystallinity. Since the mechanical properties obtained by tensile tests could not be correlated with the degree of crystallinity, detailed analysis were performed showing a characteristic inhomogeneous morphology within the tensile bars. By means of micromechanical investigations on samples with different microstructure ranges, the relationship between local morphology and failure behavior could be explained.
  • Item
    Influence of the Reaction Injection Moulding Process on the Thermomechanical Behaviour of Fast Curing Polyurethane
    (Basel : MDPI, 2022) Lehmenkühler, Peter; Stommel, Markus
    In this contribution, the influence of the reaction injection moulding process on the thermomechanical material behaviour of aliphatic hexamethylene diisocyanate (HDI) based fast curing polyurethane is demonstrated. Uniaxial tensile tests, temperature-frequency dependent dynamic mechanical thermal analysis (DMTA) and Differential Scanning Calorimetry (DSC) are used to show the differences in properties for ten different sets of process parameters. The mould and resin components temperature, the mass flow during the filling process and the residence time during the reaction process of the polyurethane are varied in several stages. Further experiments to determine the molar mass of the molecular chain between two crosslinking points of the polyurethane are used to explain the process influences on the thermomechanical properties. Thus, a direct correlation between manufacturing and material properties is shown. In addition, the mutual effect of the different parameters and their overall influence on the material behaviour is presented.
  • Item
    Determination of Strain Limits for Dimensioning Polyurethane Components
    (Basel : MDPI, 2021) Stanko, Michael; Lehmenkühler, Peter; Stommel, Markus
    Within the scope of this contribution, a method for the determination of a strain limit for designing components made of elastomeric polyurethane systems is presented. The knowledge of a material-specific strain limit is essential for the structural-mechanical calculation of plastic components in the context of component design. Compared to a commonly used component design, based on a simplified dimensioning approach taking only linear viscoelastic deformations into account, the strain limit determined in this study allows an improved utilisation of lightweight construction potential in the dimensioning of technical components made of polyurethanes through the consideration of permissible nonlinear viscoelastic deformations. The test method comprises a sequence of quasi-static loading and unloading cycles, with a subsequent load-free recovery phase, allowing the relaxation of the viscoelastic forces. Standardised tensile and simple shear test specimens and a dynamic mechanical thermal analyser (DMTA) are used within the tests. The strain limit is determined by means of the so-called residual energy ratio, which is a characteristic quantity for the evaluation of hystereses of load–unload cycles. These hystereses are increasingly formed by deformations outside the range of linear viscoelastic deformations. The residual energy ratio relates the proportion of deformation energy recovered during unloading to the deformation work that is applied. In this contribution, the residual energy ratio is successfully used to detect a significant evolution of loss energy under increasing load and to correlate this transition to a characteristic strain. The latter is used as a dimensioning parameter for the design of components made of elastomeric polyurethane materials for quasi-static load cases. The determination of this strain limit is performed under consideration of the criterion of reversibility of deformation.
  • Item
    Process Monitoring of a Vibration Dampening CFRP Drill Tube in BTA deep hole drilling using Fibre-Bragg-Grating Sensors
    (Amsterdam [u.a.] : Elsevier, 2022) Summa, Jannik; Michel, Sebastian; Kurkowski, Moritz; Biermann, Dirk; Stommel, Markus; Herrmann, Hans-Georg
    The large tool length in BTA deep hole drilling often leads to strong torsional vibrations of the tool system, leading to a reduced bore hole quality failures. When substituting steel drill tubes with tubes from composite material, the laminate structure dampens these vibrations. Secondly, the integration of sensors allow to monitor process vibrations. This contribution introduces a new sensor platform to measure process vibrations, feed force and drilling torque using Fibre-Bragg Grating Sensors. The presented experimental results focus on characteristic frequency spectra with natural torsional and compression frequencies of the CFRP drill tube, which show variations due to changed feed.
  • Item
    Prediction of Short Fiber Composite Properties by an Artificial Neural Network Trained on an RVE Database
    (Basel : MDPI, 2021) Breuer, Kevin; Stommel, Markus
    In this study, an artificial neural network is designed and trained to predict the elastic properties of short fiber reinforced plastics. The results of finite element simulations of three-dimensional representative volume elements are used as a data basis for the neural network. The fiber volume fraction, fiber length, matrix-phase properties, and fiber orientation are varied so that the neural network can be used within a very wide range of parameters. A comparison of the predictions of the neural network with additional finite element simulations shows that the stiffnesses of short fiber reinforced plastics can be predicted very well by the neural network. The average prediction accuracy is equal or better than by a two-step homogenization using the classical method of Mori and Tanaka. Moreover, it is shown that the training of the neural network on an extended data set works well and that particularly calculation-intensive data points can be avoided without loss of prediction quality.
  • Item
    Spinning of Endless Bioactive Silicate Glass Fibres for Fibre Reinforcement Applications
    (Basel : MDPI, 2021) Eichhorn, Julia; Elschner, Cindy; Groß, Martin; Reichenbächer, Rudi; Herrera Martín, Aarón X.; Prates Soares, Ana; Fischer, Heilwig; Kulkova, Julia; Moritz, Niko; Hupa, Leena; Stommel, Markus; Scheffler, Christina; Kilo, Martin
    Bioactive glasses have been used for many years in the human body as bone substitute. Since bioactive glasses are not readily available in the form of endless thin fibres with diameters below 20 µm, their use is limited to mainly non-load-bearing applications in the form of particles or granules. In this study, the spinnability of four bioactive silicate glasses was evaluated in terms of crystallisation behaviour, characteristic processing temperatures and viscosity determined by thermal analysis. The glass melts were drawn into fibres and their mechanical strength was measured by single fibre tensile tests before and after the surface treatment with different silanes. The degradation of the bioactive glasses was observed in simulated body fluid and pure water by recording the changes of the pH value and the ion concentration by inductively coupled plasma optical emission spectrometry; further, the glass degradation process was monitored by scanning electron microscopy. Additionally, first in vitro experiments using murine pre-osteoblast cell line MC3T3E1 were carried out in order to evaluate the interaction with the glass fibre surface. The results achieved in this work show up the potential of the manufacturing of endless bioactive glass fibres with appropriate mechanical strength to be applied as reinforcing fibres in new innovative medical implants.