2 results
Search Results
Now showing 1 - 2 of 2
- ItemSurviving the surf: The tribomechanical properties of the periostracum of Mytilus sp(Amsterdam : Elsevier, 2014) Wählisch, Felix C.; Peter, Nicolas J.; Torrents Abad, Oscar; Oliveira, Mariana V.G.; Schneider, Andreas S.; Schmahl, Wolfgang; Griesshaber, Erika; Bennewitz, RolandWe investigated the friction and wear behavior as well as the mechanical properties of the periostracum of Mytilus sp. Tribological properties were determined with a reciprocal sliding microtribometer, while mechanical characterization was performed using a nanoindenter. Measurements were performed in dry and wet conditions. On the dry periostracum we found a low friction coefficient of 0.078 ± 0.007 on the young parts and a higher one of 0.63 ± 0.02 on the old parts of the shell. Under wet, saline, conditions we only observed one average coefficient of friction of 0.37 ± 0.01. Microscopic ex situ analysis indicated that dry periostracum wore rather rapidly by plowing and fatigue, while it exhibited a high wear resistance when immersed in salt water. The Young’s modulus and hardness of the periostracum were also investigated in both dry and wet conditions. Under dry conditions the Young’s modulus of the periostracum was 8 ± 3 GPa, while under wet conditions it was 0.21 ± 0.05 GPa. The hardness of dry periostracum samples was 353 ± 127 MPa, whereas the hardness of wet samples was 5 ± 2 MPa. It was found that, in the wet state, viscous behavior plays a significant role in the mechanical response of the periostracum. Our results strongly indicate that the periostracum can provide an important contribution to the overall wear resistance of Mytilus sp. shell.
- ItemMechanical Characterization of Compact Rolled-up Microtubes Using In Situ Scanning Electron Microscopy Nanoindentation and Finite Element Analysis(Weinheim : Wiley-VCH, 2021) Moradi, Somayeh; Jöhrmann, Nathanael; Karnaushenko, Dmitriy D.; Zschenderlein, Uwe; Karnaushenko, Daniil; Wunderle, Bernhard; Schmidt, Oliver G.Self-assembled Swiss-roll microstructures (SRMs) are widely explored to build up microelectronic devices such as capacitors, transistors, or inductors as well as sensors and lab-in-a-tube systems. These devices often need to be transferred to a special position on a microchip or printed circuit board for the final application. Such a device transfer is typically conducted by a pick-and-place process exerting enormous mechanical loads onto the 3D components that may cause catastrophic failure of the device. Herein, the mechanical deformation behavior of SRMs using experiments and simulations is investigated. SRMs using in situ scanning electron microscopy (SEM) combined with nanoindentation are characterized. This allows us to mimic and characterize mechanical loads as they occur in a pick-and-place process. The deformation response of SRMs depends on three geometrical factors, i.e., the number of windings, compactness of consecutive windings, and inner diameter of the microtube. Nonlinear finite element analysis (FEA) showing good agreement with experiments is performed. It is believed that the insights into the mechanical loading of 3D self-assembled architectures will lead to novel techniques suitable for a new generation of pick-and-place machines operating at the microscale. © 2021 The Authors. Advanced Engineering Materials published by Wiley-VCH GmbH