Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
dc.bibliographicCitation.firstPage | 7048 | eng |
dc.bibliographicCitation.issue | 22 | eng |
dc.bibliographicCitation.journalTitle | Materials | eng |
dc.bibliographicCitation.volume | 14 | eng |
dc.contributor.author | Wang, Pei | |
dc.contributor.author | Lei, Yang | |
dc.contributor.author | Qi, Jun-Fang | |
dc.contributor.author | Yu, Si-Jie | |
dc.contributor.author | Setchi, Rossitza | |
dc.contributor.author | Wu, Ming-Wei | |
dc.contributor.author | Eckert, Jürgen | |
dc.contributor.author | Li, Hai-Chao | |
dc.contributor.author | Scudino, Sergio | |
dc.date.accessioned | 2021-12-03T13:57:36Z | |
dc.date.available | 2021-12-03T13:57:36Z | |
dc.date.issued | 2021 | |
dc.description.abstract | In this study, the wear behavior of a heat-treatable Al-7Si-0.5Mg-0.5Cu alloy fabricated by selective laser melting was investigated systematically. Compared with the commercial homogenized AA2024 alloy, the fine secondary phase of the SLM Al-Cu-Mg-Si alloy leads to a low specific wear rate (1.8 ± 0.11 × 10-4 mm3(Nm)-1) and a low average coefficient of friction (0.40 ± 0.01). After the T6 heat treatment, the SLM Al-Cu-Mg-Si alloy exhibits a lower specific wear rate (1.48 ± 0.02 × 10-4 mm3(Nm)-1), but a similar average coefficient of friction (0.34 ± 0.01) as the heat-treated AA2024 alloy. Altogether, the SLM Al-3.5Cu-1.5Mg-1Si alloy is suitable for the achievement of not only superior mechanical performance, but also improved tribological properties. | eng |
dc.description.version | publishedVersion | eng |
dc.identifier.uri | https://oa.tib.eu/renate/handle/123456789/7631 | |
dc.identifier.uri | https://doi.org/10.34657/6678 | |
dc.language.iso | eng | eng |
dc.publisher | Basel : MDPI | eng |
dc.relation.doi | https://doi.org/10.3390/ma14227048 | |
dc.relation.essn | 1996-1944 | |
dc.rights.license | CC BY 4.0 Unported | eng |
dc.rights.uri | https://creativecommons.org/licenses/by/4.0/ | eng |
dc.subject.ddc | 600 | eng |
dc.subject.other | Al-Si-Cu-Mg alloy | eng |
dc.subject.other | heat treatment | eng |
dc.subject.other | microstructure | eng |
dc.subject.other | selective laser melting | eng |
dc.subject.other | wear behavior | eng |
dc.title | Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting | eng |
dc.type | Article | eng |
dc.type | Text | eng |
tib.accessRights | openAccess | eng |
wgl.contributor | IFWD | eng |
wgl.subject | Ingenieurwissenschaften | eng |
wgl.type | Zeitschriftenartikel | eng |
Files
Original bundle
1 - 1 of 1
Loading...
- Name:
- materials-14-07048-v2.pdf
- Size:
- 3.32 MB
- Format:
- Adobe Portable Document Format
- Description: