Design of Energy and Environmentally Friendly Fiberglass Compositions Derived from the Quaternary SiO₂-Al₂O₃-CaO-MgO Phase Diagram - Part II: Fluorine-Free E-Glass Compositions Containing Low Levels of B₂O₃ and Li₂O

dc.bibliographicCitation.firstPage170
dc.bibliographicCitation.journalTitleGlass Science and Technology
dc.bibliographicCitation.lastPage183
dc.bibliographicCitation.volume77c
dc.contributor.authorWallenberger, F. T.
dc.contributor.authorHicks, R. J.
dc.contributor.authorBierhals, A. T.
dc.date.accessioned2024-08-23T15:03:30Z
dc.date.available2024-08-23T15:03:30Z
dc.date.issued2004
dc.description.abstractIncumbent E-Glass compositions contain 6 8% B₂O₃ and 0.1-1.0% fluorine. Partial emissions of these ingredients from commercial melt furnaces were recently identified as environmental hazards. Removal of all fluorine and of essentially all boron was required. But the resulting boron-and fluorine-free E-glass compositions posed another environmental concern. They had higher melt viscosities and fiber forming temperatures, and needed much more process energy. Second and thirdgeneration fluorine-free E-glass compositions were therefore developed, which contained low levels of either B₂O₃ or Li₂O and had a 26°C to 47°C lower forming temperature than optimum first generation compositions. This paper provides a detailed description of third-generation fluorine-free E-glass compositions, which contain low levels of both B₂O₃ and Li₂O, have a 65°C lower forming temperature than optimum first generation boron and fluorine-free E-glass, and promise to offer major process energy savings.eng
dc.description.versionpublishedVersion
dc.identifier.urihttps://oa.tib.eu/renate/handle/123456789/14896
dc.identifier.urihttps://doi.org/10.34657/13918
dc.language.isoeng
dc.publisherOffenbach : Verlag der Deutschen Glastechnischen Gesellschaft
dc.relation.issn0946-7475
dc.rights.licenseCC BY 3.0 DE
dc.rights.urihttps://creativecommons.org/licenses/by/3.0/de/
dc.subject.ddc660
dc.subject.gndKonferenzschrift
dc.titleDesign of Energy and Environmentally Friendly Fiberglass Compositions Derived from the Quaternary SiO₂-Al₂O₃-CaO-MgO Phase Diagram - Part II: Fluorine-Free E-Glass Compositions Containing Low Levels of B₂O₃ and Li₂Oeng
dc.typeArticle
dc.typeText
tib.accessRightsopenAccess
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
gtb77c-170.pdf
Size:
4.46 MB
Format:
Adobe Portable Document Format
Description: