    Charge carrier density, mobility, and Seebeck coefficient of melt-grown bulk ZnGa2O4 single crystals
    (New York, NY : American Inst. of Physics, 2020) Boy, Johannes; Handwerg, Martin; Mitdank, Rüdiger; Galazka, Zbigniew; Fischer, Saskia F.
    The temperature dependence of the charge carrier density, mobility, and Seebeck coefficient of melt-grown, bulk ZnGa2O4 single crystals was measured between 10 K and 310 K. The electrical conductivity at room temperature is about σ = 286 S/cm due to a high electron concentration of n = 3.26 × 1019 cm−3 caused by unintentional doping. The mobility at room temperature is μ = 55 cm2/V s, whereas the scattering on ionized impurities limits the mobility to μ = 62 cm2/Vs for temperatures lower than 180 K. The Seebeck coefficient relative to aluminum at room temperature is SZnGa2O4−Al = (−125 ± 2) μV/K and shows a temperature dependence as expected for degenerate semiconductors. At low temperatures, around 60 K, we observed the maximum Seebeck coefficient due to the phonon drag effect. © 2020 Author(s). All article content, except where otherwise noted, is licensed under a Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
  • Item
    Semimetal to semiconductor transition in Bi/TiO2 core/shell nanowires
    (Cambridge : Royal Society of Chemistry, 2021) Kockert, M.; Mitdank, R.; Moon, H.; Kim, J.; Mogilatenko, A.; Moosavi, S.H.; Kroener, M.; Woias, P.; Lee, W.; Fischer, S.F.
    We demonstrate the full thermoelectric and structural characterization of individual bismuth-based (Bi-based) core/shell nanowires. The influence of strain on the temperature dependence of the electrical conductivity, the absolute Seebeck coefficient and the thermal conductivity of bismuth/titanium dioxide (Bi/TiO2) nanowires with different diameters is investigated and compared to bismuth (Bi) and bismuth/tellurium (Bi/Te) nanowires and bismuth bulk. Scattering at surfaces, crystal defects and interfaces between the core and the shell reduces the electrical conductivity to less than 5% and the thermal conductivity to less than 25% to 50% of the bulk value at room temperature. On behalf of a compressive strain, Bi/TiO2 core/shell nanowires show a decreasing electrical conductivity with decreasing temperature opposed to that of Bi and Bi/Te nanowires. We find that the compressive strain induced by the TiO2 shell can lead to a band opening of bismuth increasing the absolute Seebeck coefficient by 10% to 30% compared to bulk at room temperature. In the semiconducting state, the activation energy is determined to |41.3 ± 0.2| meV. We show that if the strain exceeds the elastic limit the semimetallic state is recovered due to the lattice relaxation.