Development of bioactive glass-ceramics

Loading...
Thumbnail Image
Date
2004
Volume
77c
Issue
Journal
Series Titel
Book Title
Publisher
Offenbach : Verlag der Deutschen Glastechnischen Gesellschaft
Link to publishers version
Abstract

Α bioactive glass-ceramic with rhenanite, NaCaPO₄, was developed in the SiO₂ - Na₂O - CaO - P₂O₅ - F System. Crystallization and microstructure were determined by room temperature X-ray diffraction (RT-XRD) and scanning electron microscopy (SEM) methods. The surface properties of the monolithic material and its surface reactivity were investigated after immersion in simulated body fluid (SBF) for 1 to 10 days. The layer that formed was identified as hydroxyapatite (HA) using surface sensitive analytical methods. Ion exchange processes of Ca²⁺ and phosphate ions were determined. HA formed on the surface of the samples within 48 hours. An open-porous scaffold was prepared using the polymer sponge method. Based on the main results of the investigation, we conclude that rhenanite glass-ceramics possess very good bioactive properties.

Description
Keywords
Citation
Apel, E., Höland, W., & Rheinberger, V. (2004). Development of bioactive glass-ceramics. 77c.
License
CC BY 3.0 DE