Fabrication of SiO2 glass fibres by thermoplastic extrusion

Loading...
Thumbnail Image
Date
2004
Volume
77
Issue
Journal
Glass Science and Technology
Series Titel
Book Title
Publisher
Offenbach : Verlag der Deutschen Glastechnischen Gesellschaft
Link to publishers version
Abstract

The fabrication of silica glass fibres by thermoplastie extrusion of nanosize and micron SiO2 powders has been investigated. The powders were mixed with a binder system, compounded for 3 h at 150 °C, and finally extruded through a die with a 500 μm-diameter die land. After debinding the green fibres at 500 °C, these were sintered for 1 h at 1100°C under air to yield glassy and crack-free silica fibres with a final diameter of 400 μm. The effect of the two different particle size distributions as well as the influence of varying powder loading (between 38 and 58 vol.%) on the rheological properties of the feedstocks were analysed using capillary rheometry. The debinding and sintering behaviour was also investigated using mercury intrusion porosimetry, thermal gravimetrie analysis and dilatometry.

Description
Keywords
Citation
Heiber, J., Clemens, F., Graule, T., & Hülsenberg, D. (2004). Fabrication of SiO2 glass fibres by thermoplastic extrusion. Offenbach : Verlag der Deutschen Glastechnischen Gesellschaft.
License
CC BY 3.0 DE