Nickel sulphide: supplementary statistical data of the heat soak test

Loading...
Thumbnail Image

Date

Volume

73

Issue

Journal

Glass Science and Technology

Series Titel

Book Title

Publisher

Offenbach : Verlag der Deutschen Glastechnischen Gesellschaft

Link to publishers version

Abstract

Supplementary heat soak test (HST) breakage data completing those recently published are in good agreement with the latter. The overall evaluation of the whole data set for one type of HST oven with a big number of recorded break events shows that a holding time of 2 h at (290 ± 10) °C is enough to ensure sufficient reliability of the test.